The Ultimate Guide To trafo starlite
Blow-out failure: failure is characterised because of the lateral spalling of concrete within the proximity with the anchor's head. This type of failure takes place for anchors (prevalently Forged-in-location) mounted near the edge with the concrete aspect.Steel failure: the rod reaches the yielding capacity then rupture happens right after develop